Default adding graphics to powder coating

Is it possible to get a special decal made that is heat resistant, and powder coat over it with a clear coat to add graphics to a piece? Thanks.


Please let me know if you have any ideas.
Reply With Quote
  #2 (permalink)  
Old 03-20-2005, 10:19 AM
Newbie
 
Join Date: Mar 2005
Posts: 16
KeithLambert7
Default

Can't vouch for them, but Victory Circle Graphics makes them. I would imagine the graphics would stand 'proud' of the surface after the clearcoating, vs. during solvent painting, the surface is wetsanded after the clear is applied to bring the two surfaces together.

I can't figure out how you'd do that with PC sinces it's not really a wet-sandable process?? Anyone know?

Keith
Reply With Quote
  #3 (permalink)  
Old 03-20-2005, 11:12 PM
Amateur Metal Finisher
 
Join Date: Dec 2004
Location: Overland Park Ks
Posts: 89
kchotboat
Default

what you need is to buy a sheet of the same material as the green tape and take it to a decal shop and have it cut out.
Reply With Quote
  #4 (permalink)  
Old 03-21-2005, 01:22 AM
11111111's Avatar
Amateur Metal Finisher
 
Join Date: Nov 2003
Location: washington state
Posts: 167
11111111
Send a message via MSN to 11111111 Send a message via Yahoo to 11111111
Default

my brother just bought a vinyl sign machine and we found stuff that does 350f. what were going to do is make logos and place them over a cured base coat and re shoot with a new color and pull the sticker up and bake. should leave a cool logo. the soft ware is also used for a four color sreen printing set up. with this and mulitpe cure cylcles we should be able to do what ever you can do for a tee shirt with a four color screen print. this way we can use the cheapest vinyl and heat wot be a issue. FYI
__________________
Thier are only two real sports!
boxing and auto racing
all the rest are just games.

Drive it like you stole it!
Reply With Quote
  #5 (permalink)  
Old 10-06-2005, 09:38 PM
Newbie
 
Join Date: Oct 2005
Location: Minnesota
Posts: 28
PowderVisions is on a distinguished road
Default Re: adding graphics to powder coating

Many decal makers have the ability to make you high temperature decals that you can apply a clear topcoat over. Both Harley and Excelsior-Henderson did this. Excelsior-Henderson applied acrylic clear over their decals and they look great.
Reply With Quote
  #6 (permalink)  
Old 10-07-2005, 11:24 PM
Experienced Metal Finisher
 
Join Date: Apr 2004
Posts: 466
jtagger19 is on a distinguished road
Default Re: adding graphics to powder coating

you can wet sand and polish powder coating
I've done this to eliminate some wavy finishes and scratches on old powder coatings .
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
*** WE ARE GIVING AWAY FREE POWDER COATING *** mcaswell Powder Coating Questions 197 07-08-2008 12:31 PM
powder coating over powder coat? corybarta Powder Coating Questions 6 08-21-2006 08:15 AM
Powder coating on firearms LoneGunman Powder Coating Questions 2 06-15-2006 12:54 PM
IR heater for powder coating questions dagobert Powder Coating Questions 1 06-12-2004 08:57 PM
Non-paint powder coating dshepherd Powder Coating Questions 6 01-26-2004 11:49 AM


All times are GMT -4. The time now is 11:53 AM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.