Plating Powder Coating Buffing Anodizing - Caswell Inc. Metal Finishing Forum  

Go Back   Plating Powder Coating Buffing Anodizing - Caswell Inc. Metal Finishing Forum > Powder Coating Questions

Notices

Powder Coating Questions Discussion Board For powder coating questions.

FREE POWDER COATING SYSTEM

Until 9/15 - Buy an HV System, Get a Regular PC System FREE! Two systems for the price of one! (Limited Time - US Customers Only)

HV Powder Coating System

Buy Now


Reply
 
Thread Tools Display Modes
  #1 (permalink)  
Old 03-28-2005, 04:26 PM
getastro's Avatar
Amateur Metal Finisher
 
Join Date: May 2003
Location: NSB, FL.
Posts: 59
getastro
Default Question for the guys out there with gas ovens

Okay, I am switching from electric to gas and I am wondering how much gas does your ovens use and the size of it. I am have problems getting gas piped into the house, but with the right amount of money or high amount of gas they will pipe it in for sure. The other option is a large tank I am thinking around 250gal, but problems there to. Just looking to see how the gas ovens are feed. By the way I am thinking of using an propane forced air heater, running around 225k BTU Per Hour.
Reply With Quote
  #2 (permalink)  
Old 03-28-2005, 09:07 PM
KZjim's Avatar
Amateur Metal Finisher
 
Join Date: Oct 2004
Location: Cereal City - There's a lot of flakes here
Posts: 132
KZjim is on a distinguished road
Send a message via Yahoo to KZjim
Default

im in the process of building a propane powered oven, i should be completed in 2 weeks or so... ill post pics and any other info i can... it's a tank that is 5' long and 3' in diameter.
__________________
If it jams; Force it. And if it breaks it needed replacing anyway.

I can go from 0 to "What seems to be the problem Officer?" in 3 seconds."
Reply With Quote
  #3 (permalink)  
Old 03-30-2005, 07:17 PM
Newbie
 
Join Date: Feb 2004
Posts: 35
Jay87T
Default

I have a Gas oven works really good, I made it myself its about 4 cubic feet, I used a BBQ burner on the bottom and I heat it up to 420 and cook my parts. as for propane usage, it lasts a very long time,
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Ovens with gas question getastro Powder Coating Questions 22 11-08-2004 12:06 PM


All times are GMT -4. The time now is 12:22 AM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.