neon
Default Military Blue Wrinkle ( not wrinkling)

I have tried several differant cure times and temps with blue wrinkle and cannot get this stuff to wrinkle. It comes out glossy everytime.. I consulted a friend that has lots of coating experience, He also has tried 5 or 6 samples to seeif he could get it to work he could not... Please Advise i need to get these parts out to my customer ASAP.. Thanks guys
Reply With Quote
  #2 (permalink)  
Old 04-04-2005, 11:16 PM
sswee's Avatar
Moderator
 
Join Date: Nov 2004
Location: close to Austin, Texas
Posts: 1,212
sswee is a jewel in the roughsswee is a jewel in the roughsswee is a jewel in the roughsswee is a jewel in the rough
Default

Quote:
This is Caswell's Black Wrinkle powder.
I cured it at 375 for 15min.
When I did it at 400deg. the powder would turn to a gloss black with no wrinkle to it at all.
This is a post from Warchild on page 2. Maybe this will help. There were some with the same problem with the black wrinkle.
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
wrinkle not wrinkling jtagger19 Powder Coating Questions 6 10-06-2005 07:17 PM
Black Wrinkle warchild Powder Coating Questions 4 03-18-2005 06:52 PM
Caswell Blue 4A PhilM Anodizing Questions 3 01-27-2005 09:23 PM
Red vs Blue vs Brown for gold and silver c_gismo Metal Polishing Questions 3 11-11-2003 05:17 PM
Blue Anodize keith_a_bond Electroplating Questions 1 03-03-2002 07:30 PM


All times are GMT -4. The time now is 11:28 PM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.