I beg to differ. A long ways back I mixed a glossy black and a glossy red and got a glossy burgundy. I even added more glossy black and came up with a dark red or as I call it CHOCOLATE!
My friend mixed a translucent copper and dark silver texture and came out with a hint of copper and silver beauty. This he did to his motorcycle headlight cover:
|
|
|||
|
This could be a good post to come up with something new, new type of colors and post the results. I am going to try mixing black onyx and gloss black to see what I come up with . Also going to mix up some metalic silver and the candy blue top coat. I also may try mixing ribbon blue with the blue candy top coat. Very interesting. I will let you know how it all works. I can now see I may have to get myself a digital camera to post some pics, later guys
|
|
||||
|
I mixed red and yellow together and came up with a sick orange...chuck...found the package that my boy was supposed to take to ups to you monday in his truck still.i'll get it on its way this monday..
__________________
Pro-Tech Powder Coating 93976 Ocean Way 541-247-8168 protech@harborside.com Gold Beach,Oregon |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| MIXING POWDERS | turch | Powder Coating Questions | 7 | 12-01-2004 11:00 PM |
| types of powders | sportster883r | Powder Coating Questions | 3 | 11-20-2004 10:57 PM |
| Clear coat over Illusion powders? | abyss33 | Powder Coating Questions | 2 | 07-05-2004 12:50 PM |
| what are similar powders from caswell to eastwood | pghmerlin69 | Powder Coating Questions | 6 | 02-26-2004 03:39 PM |
| which powders ? | duke | Powder Coating Questions | 1 | 09-27-2003 03:22 PM |