why i was doing my upper a arms i sprayed white baked it let the part get too 120 130 or so then went over it with tropical orange and got tropical poo it looked like when u put put paint stripper on something before u strip it on the one side and i put a good coating on and it still didnt look like it covered evenly and how do u prep the peice for recoating thanx
|
|
|||
|
you can put the part in a oven and set it at clean 800F this should aid in the removal by baking it off. to prep after coated . I use a sharp oxide ot steel to remove it. it is best to remove if you have alot of defects in the coating .
Good luck. and happy powdering :' Chuck |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| powder coating over powder coat? | corybarta | Powder Coating Questions | 6 | 08-21-2006 08:15 AM |
| Finding a place to powder coat | RCLSolutions | Powder Coating Questions | 3 | 05-04-2005 09:42 PM |
| Powder Coat caught on fire! | Sleepr_Tech | Powder Coating Questions | 3 | 09-10-2004 06:22 AM |
| Laser printer = Powder Coat Printer? | tbloss001 | Powder Coating Questions | 11 | 08-30-2004 06:08 PM |
| Magnesium-sticking powder coat to it and the cleaning proces | fst951 | Powder Coating Questions | 5 | 04-14-2004 01:53 AM |