  #1 (permalink)  
Old 04-24-2005, 04:22 PM
Newbie
 
Join Date: Dec 2004
Posts: 34
chicagorich
Default out gassing questions?

I prebake all my parts 550 degrees for 1 hour to reduce out gassing and have had good results. When my cure time is up i open up my top access panel to inspect the piece and they look perfect. When i pull out the piece its great then like a minute later outgassing bubbles start poping out here and there right before my eyes. Any body have an idea of whats going on?
Reply With Quote
  #2 (permalink)  
Old 04-24-2005, 05:52 PM
hvac36's Avatar
Moderator
 
Join Date: Jul 2004
Location: New Milford, PA
Posts: 219
hvac36 will become famous soon enough
Send a message via AIM to hvac36
Default

Here is how I do it.
Pre-Heat to 450 or 50 degrees above my Cure Temp, let part cool to 150 +/- degrees then powder. Cure at 375 for time spec'd per powder. Let cool in Oven down to 200 degrees then remove.. Never had a problem with out gassing...

Jim S...
__________________
Jim Shuster
www.backyardpowdercoating.com Sold.....
www.chrissys68mustang.com Hobbie
www.photogserver.net Web Hosting.
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Some newbie questions... kiwijetpilot Anodizing Questions 16 03-12-2005 08:18 PM
First time anodizing questions scocklin Anodizing Questions 10 12-04-2004 04:45 AM
Questions from a new member of this forum msaffer Electroplating Questions 2 10-04-2004 01:44 AM
A few newbe questions thestormfamily Electroplating Questions 4 06-30-2004 08:54 AM
Newbie with many questions about annodizing paintball guns. djisrael1 Anodizing Questions 10 11-11-2002 08:28 PM


All times are GMT -4. The time now is 12:59 AM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.