I try to use black wrinkle and if the part is left more than 5 minutes the wrinkles will melt and all I get is gloss black
I tried curring at 380 and at 400 and the same thing happend . anyone else have had this problem
|
|
|||
|
Didnt have any problem here. Looks great! Put parts in cold. Turned oven on to 400 degress... took about 12 minutes to get to temp/melting look. Then waited another 14 minutes. Let cool with the the door cracked open.
Perfect! |
|
|||
|
The only time I've ever had problems with a wrinkle was b/c a blocking agent was being released by another powder I was running and it just killed the wrinkle... A good article on troubleshooting wrinkle finishes:
http://www.rohmhaas.com/powdercoatin...s_wrinkle.html |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Military Blue Wrinkle ( not wrinkling) | neon | Powder Coating Questions | 1 | 04-04-2005 11:16 PM |
| Black Wrinkle | warchild | Powder Coating Questions | 4 | 03-18-2005 06:52 PM |
| super chrome wrinkling | jtagger19 | Powder Coating Questions | 8 | 02-07-2005 10:15 PM |
| Which HB Fuller Color is Robin Red Wrinkle? | Noob2PC | Powder Coating Questions | 2 | 04-22-2004 07:43 PM |
| Wrinkle finish | matrob | Powder Coating Questions | 7 | 07-22-2003 08:10 PM |