has anybody used the glow in the dark additive (pcppsa3) with safety orange (pcp56002) will it work well together and glow?
What about the glow in the dark additive (pcppsa3) with the neon green(pcppss1221) any help on this would be great |
|
|||
|
Ive used glow in the dark over candy blue, candy red, white ,candy yellow and it always works
the diference is the time it glows and the amount it glows the lighter the color the more time it will glow . so I think it will work over saftey orange with no problems. |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Glow in the Dark | PhilM | Powder Coating Questions | 6 | 01-28-2005 02:52 PM |
| glow in the dark powder? | upncoming | Powder Coating Questions | 5 | 06-27-2004 01:50 PM |
| Make Your Parts Glow | mcaswell | Powder Coating Questions | 8 | 04-05-2004 06:00 AM |
| Glow | warchild | Powder Coating Questions | 4 | 06-29-2003 02:52 PM |
| How dark is the olive drab? + zinc question. | jbvan | Electroplating Questions | 4 | 02-01-2003 01:12 AM |