Just curious who makes these powders for Caswell?
Reply With Quote
  #2 (permalink)  
Old 05-19-2005, 10:22 PM
customandsound
Guest
 
Posts: n/a
Default

if you contact caswell tech they may tell you..
Reply With Quote
  #3 (permalink)  
Old 05-20-2005, 09:22 AM
mcaswell's Avatar
Caswell Inc Founder
 
Join Date: Nov 2001
Location: Lyons, NY USA
Posts: 2,357
Blog Entries: 1
mcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to behold
Default

We use a number of different suppliers. HB Fuller is the main one, also NIC, DuPont and Tiger Drylac (sson)
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Reply With Quote
  #4 (permalink)  
Old 05-20-2005, 09:56 PM
customandsound
Guest
 
Posts: n/a
Default

I just did not want to let the cat out of the bag if you know what i am saying . But all of those companyes sell some great powder i dealt with them one time or another but you need to buy bulk50lb
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Caswell Please Call Me, I AM A BUYER Brad_Davis Metal Polishing Questions 4 12-05-2004 01:30 AM
1st job w/ Caswell powder nuttyman Powder Coating Questions 2 06-03-2004 07:42 PM
what are similar powders from caswell to eastwood pghmerlin69 Powder Coating Questions 6 02-26-2004 03:39 PM
are the Caswell powders resistant to acetone or xylene? tbloss001 Powder Coating Questions 3 09-14-2003 03:55 PM
Manufacturer of Powder from Caswell and Hotcoat Fireblade Powder Coating Questions 5 06-11-2003 12:29 PM


All times are GMT -4. The time now is 09:03 AM.


Powered by vBulletin® Version 3.7.4
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0
Copyright © Caswell Inc.