do they need to be applied over chrome to get that nice shiny look ? can i just apply them over a sand blasted atv frame ? if not can i powder coat chrome then powder over that with the candy color to get the nice shiny effect.
|
|
|||
|
You probably need to put a base coat of chrome powder, then the candy color. A white, silver or aluminum base color also looks good under most candy colors.
Leo
__________________
www.tinmans.net "Life is not a journey to the grave with the intention of arriving safely in a pretty and well preserved body, but rather to skid in broadside, thoroughly used up, totally worn out, and loudly proclaiming -- WOW--What a Ride!!!" ----- Unknown |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| candy candy candy looks hot! | 11111111 | Powder Coating Questions | 8 | 03-12-2005 02:26 AM |
| Couple questions... (candy, hi-temp) | epix | Powder Coating Questions | 1 | 02-12-2005 09:18 AM |
| candy color? | randygrapes218 | Powder Coating Questions | 1 | 01-03-2005 12:09 AM |
| Candy Orange Powder Problems | matrob | Powder Coating Questions | 4 | 10-07-2003 07:50 AM |
| Problems with clear, flowout, multiple colors, more... | allcarfan | Powder Coating Questions | 3 | 08-25-2003 10:49 PM |