corecoatings is an unknown quantity at this point
Default Need info on powder for 67 Firebird Rally 2 rims

From what I gathered from the customer there are two color grays. One light one darker.
Anyone know which powders represent the colors for these rims.

Also after doing the triangles, he has a mask kit for them.Probably not high temp. What are the chances of leaving them and cooking then removing and wiping remains off? Any thoughts? Anyone? Powder on.........Andy
Reply With Quote
  #2 (permalink)  
Old 06-10-2005, 05:07 PM
customandsound
Guest
 
Posts: n/a
Default

them insterts will come off the wheel. gm uses a argent for the color ..

you may want to tape them off with high temp tape instead

the 3 colors gm used
silver charcoal and black

any other color was custom sprayed on
Reply With Quote
  #3 (permalink)  
Old 06-10-2005, 11:46 PM
Amateur Metal Finisher
 
Join Date: Dec 2004
Location: Freedom Vale
Posts: 167
corecoatings is an unknown quantity at this point
Default Need info on powder for 67 Firebird Rally 2 rims

So there are 3 colors?
Are those the colors you posted for powders, silver, charcoal, and black
?
Are they caswell?
I think I quoted a little low $42.00 a rim, what do you think?
Reply With Quote
  #4 (permalink)  
Old 06-11-2005, 01:43 AM
customandsound
Guest
 
Posts: n/a
Default

them colors are factory color...I charge and get 300 a set of 4 75 each 2 coats front 1 coat in the rear and 1 coat of clear
Reply With Quote
  #5 (permalink)  
Old 06-13-2005, 09:02 PM
Amateur Metal Finisher
 
Join Date: Dec 2004
Location: Freedom Vale
Posts: 167
corecoatings is an unknown quantity at this point
Default Need info on powder for 67 Firebird Rally 2 rims

So when you say factory, you are talking solvent based painting correct?
Reply With Quote
  #6 (permalink)  
Old 06-14-2005, 12:00 AM
customandsound
Guest
 
Posts: n/a
Default

give me a call tommorrow . i got tied up today or i would of called ya
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Looking for info on an unidentified powder stevevanos Powder Coating Questions 2 03-10-2005 12:34 AM
powder info drfjr1976 Powder Coating Questions 6 12-30-2003 11:53 AM


All times are GMT -4. The time now is 08:54 PM.


Powered by vBulletin® Version 3.7.4
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0
Copyright © Caswell Inc.