  #1 (permalink)  
Old 06-13-2005, 09:33 PM
Amateur Metal Finisher
 
Join Date: Dec 2004
Location: Freedom Vale
Posts: 167
corecoatings is an unknown quantity at this point
Default Taping over cured powder for a second color

Will the tape make a mess if it is left on the already cured power ie, pull it off ,melt into it.
I had an experience with taping off high gloss clear and recoloring and it pulled off the clear. I think the clear was still warm/hot.
Any thoughts, comments, anyone care for a mint?
Basically trying to find the prefered method for doing two colors. I liked the one about the two sided tape and taking it off before curing.

Powder to the people!
Reply With Quote
  #2 (permalink)  
Old 06-20-2005, 06:46 PM
Amateur Metal Finisher
 
Join Date: Dec 2004
Location: Freedom Vale
Posts: 167
corecoatings is an unknown quantity at this point
Default Nobody has taped over cured powder?

n/m
Reply With Quote
  #3 (permalink)  
Old 06-20-2005, 09:55 PM
Amateur Metal Finisher
 
Join Date: Nov 2004
Location: Mississippi Gulf Coast
Posts: 84
tinbender722 is an unknown quantity at this point
Send a message via AIM to tinbender722 Send a message via Yahoo to tinbender722
Default

I will let you know tomorrow. I have a set of valve covers and a fan blade that I coated with first color today and will tape up and spray second color tomorrow.

Leo
__________________
www.tinmans.net
"Life is not a journey to the grave with the intention of arriving safely in a pretty and well preserved body, but rather to skid in broadside, thoroughly used up, totally worn out, and loudly proclaiming -- WOW--What a Ride!!!" ----- Unknown
Reply With Quote
  #4 (permalink)  
Old 06-21-2005, 07:07 AM
Amateur Metal Finisher
 
Join Date: Dec 2004
Location: Freedom Vale
Posts: 167
corecoatings is an unknown quantity at this point
Default Taping

Not that I am too lazy to try but, I think it is a good idea try and get some solid info on the process of taping over cured powder. I know it is a whole lot better to get it off but in some cases you have to to let it ride. Tinbender I really like that quote.
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
*** WE ARE GIVING AWAY FREE POWDER COATING *** mcaswell Powder Coating Questions 197 07-08-2008 01:31 PM
powder color pickleboy Powder Coating Questions 1 07-13-2005 01:41 AM
Powder color request tavo1765 Caswell Please Sell This... 2 03-17-2005 10:53 PM
How long will the powder hold until it needs to be cured? trsick Powder Coating Questions 13 03-14-2005 01:23 PM
New Product - Illusions Powder Coating mcaswell Powder Coating Questions 1 03-11-2004 06:06 PM


All times are GMT -4. The time now is 08:52 AM.


Powered by vBulletin® Version 3.7.4
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0
Copyright © Caswell Inc.