| Notices |
| Powder Coating Questions Discussion Board For powder coating questions. |
![]() |
|
|
Thread Tools | Display Modes |
|
|||
|
Well i tryed a few types of tape today. Below is the rating.(no pics my camera in in the car )
1. Green fiber glass tape : Perfect little glue from curing 2. 3m Painters tape : Nightmare stuck like cement on block took 3 hours to remove. 3. white fiber glass cloth.. : Perfect but not cheap well to remove the cheaper 3m painters tape ( blue ) you need to get a spray bottle and put light cuts in it. then spray it down few sprays. i get it wet and wait a few minutes then spray it again. and it comes right off then a little thinner to clean it up. Now when you got a big part ( wheel) Foil or the white fiber glass cloth. I will get a few pics of this so what i am getting at DON'T try to cut corners it just give you more work and less time showing you perfect part off |
|
||||
|
I use the red polyester tape from cfs its good to 425f it comes off nice and easy...there 5 mil cloth has 3 mils of silicone adhesive and its good to 500f and comes off sweet..btw chuck sorry i missed your call..best to get me at the shop...
__________________
Pro-Tech Powder Coating 93976 Ocean Way 541-247-8168 protech@harborside.com Gold Beach,Oregon |
|
|||
|
i used it to mask off. i will be looking for other tape to test in my travels ..
that is ok. i will call the shop one day this week ..i need to call dale and see how he is doing to .. i have that number in my cell phone i was not sure if it was the house or the shop i wrote the shop number down i am going to put it on speed dail #2 #1 is my tow guys |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| hi temp tape shrinking | craigcraig | Powder Coating Questions | 10 | 11-27-2004 11:04 PM |
| high temp tape | randygrapes218 | Powder Coating Questions | 3 | 07-29-2004 08:57 PM |
| Tape for Masking | johnny933 | Powder Coating Questions | 2 | 05-11-2004 03:12 AM |
| Powder Coating Masking Tape Now Available | mcaswell | Powder Coating Questions | 0 | 08-21-2003 02:13 PM |
| Looking for masking tape recomendations. | chcarver | Metal Polishing Questions | 0 | 03-06-2003 02:51 PM |