I got a pair of valvecovers from a customer that he wants powdercoated. He wants the letter on it black, and the cover in transparent candy powder. Any tips or tricks on how to get the letters in black, need some masking tips or something. The covers looks like this:
![]() I have seen it done, just cant figure out how |
|
|||
|
the letter look deep not risen
for deep letters here is what I do I do the outside first and fully cure then tape the out side and powder the letters , remove the tape before curring the letters so you can fix any powder left where it shouldn't be. and cure the letters the problem I had doing the letters first was that once the outside was cure it builds inside the letters not allowing me to remove the tape. this is the way I've been doing it for a while now maybe some one else has a better and easier idea. |
|
|||
|
Well, found another way, put a layer of the lettercolor first, used a dry hard sponge to brush off the overflow, worked pretty good...
|
|
|||
|
I started with normalt blasting the get the old color off. Then i glass bead blasted it to get a nice finnish to it.
Then i just applied a layer of purple, just enough to cover the text, then used the sponge to remove the overflow of powder. Just drag the sponge over the cover with very little pressure, and you will get rid of the powder outside of the text. Took a few times to get it done without toughing inside the text, but it worked great once i got the hang of it. Cure it, glas bead blasted it again to remove the small dots of powder i missed to remove, and the a layer of clear over the whole cover and cured it again. |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| New Powder Colors, Sizes, and Technical Data | mcaswell | Powder Coating Questions | 13 | 06-21-2007 01:16 PM |
| Flourescent Colors | CaptainChauncy | Powder Coating Questions | 2 | 02-17-2005 06:21 PM |
| Need help..... Looking for Arctic Cat colors | Sleepr_Tech | Powder Coating Questions | 0 | 08-02-2004 08:49 PM |
| doing two colors help | boucher | Powder Coating Questions | 9 | 06-26-2004 06:00 PM |
| Problems with clear, flowout, multiple colors, more... | allcarfan | Powder Coating Questions | 3 | 08-25-2003 10:49 PM |