Old 07-09-2005, 02:04 AM
Newbie
 
Join Date: Mar 2005
Posts: 45
Deecoat
Default Gun Pressure?

Hello all, Can anyone tell me what pressure to set the gun at for coating? Are there different settings for certain objects and materials? Thanks all!
Reply With Quote
  #2 (permalink)  
Old 07-09-2005, 08:12 AM
Blademan's Avatar
Experienced Metal Finisher
 
Join Date: Mar 2004
Location: Gold Beach, Oregon
Posts: 322
Blademan is on a distinguished road
Default

8 to 10 # is normal , I adjust my regulator on the gun as needed..some times more, some times less...and if I get really frustrated i put it in hurricane mode....
__________________
Pro-Tech Powder Coating
93976 Ocean Way
541-247-8168
protech@harborside.com
Gold Beach,Oregon
Reply With Quote
  #3 (permalink)  
Old 07-09-2005, 01:12 PM
Amateur Metal Finisher
 
Join Date: Jul 2004
Location: Cape Cod Mass.
Posts: 157
trsick
Default Re: Gun Pressure

I set my air pressure at 15psi when I pull the trigger it drops to roughly 10 psi.
Works well.
Bob
__________________
www.capecodpowdercoating.com
Reply With Quote
  #4 (permalink)  
Old 07-10-2005, 01:18 AM
Newbie
 
Join Date: Mar 2005
Posts: 45
Deecoat
Default

Thanks Guys! Hope business is well!
Reply With Quote
  #5 (permalink)  
Old 07-10-2005, 04:15 AM
customandsound
Guest
 
Posts: n/a
Default

the hose holds 5lbs .. but i shoot from 8-10 depending on the powder i am shooting ....

Tip: use a moister filter.. and replace then 1 or more times a month.
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Compressor help mpierich Metal Polishing Questions 2 07-13-2005 11:29 AM
Building your own pressure pot Pearl-Jam Powder Coating Questions 3 04-03-2005 01:25 PM
proper air pressure scoober Powder Coating Questions 7 03-21-2004 05:26 PM
Air pressure darkerimages Powder Coating Questions 1 02-05-2004 07:30 PM
Air pressure ?? 208019913 Powder Coating Questions 2 07-30-2003 04:40 PM


All times are GMT -4. The time now is 08:56 PM.


Powered by vBulletin® Version 3.7.4
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0
Copyright © Caswell Inc.