Plating Powder Coating Buffing Anodizing - Caswell Inc. Metal Finishing Forum  

Go Back   Plating Powder Coating Buffing Anodizing - Caswell Inc. Metal Finishing Forum > Powder Coating Questions

Notices

Powder Coating Questions Discussion Board For powder coating questions.

Reply
 
Thread Tools Display Modes
  #1 (permalink)  
Old 07-10-2005, 08:48 PM
Amateur Metal Finisher
 
Join Date: Mar 2005
Posts: 64
Heavykote
Default Having a go at powdercoating plastic...pics

Yes guys I've decided to give plastic a try. First job, CENTERCAPS! Plastic center w/aluminum trim ring around.
Here's a pic of one with chrome powder:

Here's one I started to sandblast:

I don't have any pics with the results, but I can tell you that 400 degrees for 10 minutes doesn't work with this type of plastic.
It appears that after trying 400, 300, and 250 the 250-300 range is best. The only thing I didn't do till my last 2 caps was to heat up the adhesive under the logo,
then prying it off.
Reply With Quote
  #2 (permalink)  
Old 07-10-2005, 11:09 PM
customandsound
Guest
 
Posts: n/a
Default

i am going to do my centers. can you post a pic of the final result
Reply With Quote
  #3 (permalink)  
Old 07-11-2005, 04:19 PM
Amateur Metal Finisher
 
Join Date: Mar 2005
Posts: 64
Heavykote
Default

Definitely, but today the temps are in the 90's so I'm CHILLIN OUT!
Reply With Quote
  #4 (permalink)  
Old 07-11-2005, 05:13 PM
customandsound
Guest
 
Posts: n/a
Default

that is why i hung out in the house all day .... i am waiting til 9 or 10 to go out and powder.

Heavykote can you pm me your domain link.. i tryed to fid you car on ther to take a peek
Reply With Quote
  #5 (permalink)  
Old 07-12-2005, 09:26 PM
Amateur Metal Finisher
 
Join Date: Mar 2005
Posts: 64
Heavykote
Default

Okay, the deed is done. I ended up putting the centercap in at I think 263+ or - . Stripping the center of the cap down was a major pain, but near the end I found a easier way to do it.



The aluminum ring came out good,BUT the center plastic piece became bubbly. This I think is mostly cause of the temp and time in the oven. I think 5 to 10 miuntes is top for a piece. I was actually smoking some ribs on my day off while doing this. Big mistake, but I wasn't thinking clearly especially while drinking a couple of beers. Funny thing is the only time I drink is when I grill.
I guess my next test will be when I get more centercaps, but progress was made...
Reply With Quote
  #6 (permalink)  
Old 07-12-2005, 11:04 PM
customandsound
Guest
 
Posts: n/a
Default

they look better than i thought they would... i got flat centers for my aucra i want to color match the wheels either that i am just going to use chrome lug's
Reply With Quote
  #7 (permalink)  
Old 07-13-2005, 08:44 PM
Amateur Metal Finisher
 
Join Date: Mar 2005
Posts: 64
Heavykote
Default

I know they can be done right! I just have so much to do and so little time in a day. Right now I'm about to do a translucent red impala rim. I'll post pics when I'm done...
Reply With Quote
  #8 (permalink)  
Old 07-13-2005, 08:48 PM
customandsound
Guest
 
Posts: n/a
Default

they can be done i have seen a few flat ones done in a low cure .. i am going to color match mine charcoal met. i got to get the livestock taken care of first so i can get time for my own projects
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
powdercoating plastic engine pieces myillwillinc Powder Coating Questions 10 04-08-2005 05:58 PM
cheap powdercoating heater/chrome power supply question dagobert Electroplating Questions 0 06-01-2004 11:59 AM
Powdercoating plastic mystrwizard Powder Coating Questions 11 04-23-2004 07:38 AM
Plating clear plastic Dinosaurius Electroplating Questions 2 06-11-2003 12:06 PM
copper peeling from plastic chromeman66 Electroplating Questions 1 02-06-2003 01:35 PM


All times are GMT -4. The time now is 04:14 PM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.