Default Re: Home Garage Powder Coaters???

I have both, the Caswell and the Chicago guns. The Caswell gun seams to perfurm more consistantly.
__________________
Lee Parsons
Rowlett, TX (East Dallas)
Reply With Quote
  #22 (permalink)  
Old 09-14-2005, 12:20 PM
Newbie
 
Join Date: Aug 2005
Posts: 7
frogwash is on a distinguished road
Default Re: Home Garage Powder Coaters???

Awesome! I will pick up a Caswell and see how it works out. does anyone use a regular oven? (not in the house) But pick up an old oven ... so it's 20 minutes @ 400 degrees?

thanks

frogwash
Reply With Quote
  #23 (permalink)  
Old 09-14-2005, 02:37 PM
Newbie
 
Join Date: Jun 2005
Location: Rowlett, TX
Posts: 41
LeeParsons
Send a message via ICQ to LeeParsons
Default Re: Home Garage Powder Coaters???

An electric kitchen oven will work just fine. Some guys have even made extensions to be able to cure larger parts in kitchen ovens. Another thing about kitchen ovens is that when you get to the point of needing a larger oven you have most of the parts to build opne already.

Your powder should have the curing temp and time on the lable but generaly its 400 at 15 to 20 minutes. I have some that are 375 at 15 so make sure you check the lable.
__________________
Lee Parsons
Rowlett, TX (East Dallas)
Reply With Quote
  #24 (permalink)  
Old 11-27-2005, 09:09 AM
Amateur Metal Finisher
 
Join Date: Sep 2005
Posts: 52
coleman5 is on a distinguished road
Default Re: Home Garage Powder Coaters???

tip find an old water heater and us it as a holding tank for that small compresor works for me.
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off


All times are GMT -4. The time now is 08:40 PM.


Powered by vBulletin® Version 3.7.4
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0
Copyright © Caswell Inc.