Sorry I haven't been on here in a REAL long time, I have been lurking from time to time
I was just curious though, how much powder does a normal frame need? I plan on using my IR lamp and a couple of reflectors, any idea how long something like that might take to cure? I have been sand blasting the frame with black oxide for what seems like the past month and no matter what I do, flash rust comes around when it site overnight. Can I use a fine grit(120?) sanding sponge to get rid of the flash and clean re clean the entire thing w/ acetone before spraying? anybody else have another suggestion? Thanks for any help This is my biggest job yet so wish me luck. |
|
|||
|
For some reason, the one i just did, didn't flash rust....
I used about 1/2 lb of chrome basecoat and almost 1 lb of candy red topcoat.(not sure why it didn't go as far) This was on a Honda 250R frame. |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| PC'ing an old truck frame... | dansilbaugh | Powder Coating Questions | 5 | 07-22-2005 04:11 PM |
| Frame polishing....same process...2 different finishes? HELP | bairdmotorcycles | Metal Polishing Questions | 15 | 06-27-2005 03:13 PM |
| polishing frame | shaybirde | Metal Polishing Questions | 4 | 04-23-2005 11:18 PM |
| Frame Polishing Question | SICKGIXX | Metal Polishing Questions | 10 | 03-18-2003 10:50 AM |
| Frame frustrations | Josh | Metal Polishing Questions | 22 | 02-20-2003 11:15 PM |