Default Noob

Hello all. I am very interested in starting my own business. I am considering an Idea... How hard would it be to Create a "portable" station?

Please tell me if you think this is possible...

1.Small enclosed trailer (insulated) with strategic curing lamps.
2.Air compressor
3. Parts cleaner

I know there are other things but I guess my Question is could a trailer double as a blast booth and a spray booth?

Also My trailer would require adequate ventilation as well.


CAN IT BE DONE

if you have any Ideas email me At chris_hale007@yahoo.com
Reply With Quote
  #2 (permalink)  
Old 10-12-2005, 10:26 PM
Amateur Metal Finisher
 
Join Date: Aug 2004
Posts: 68
CaptainChauncy is an unknown quantity at this point
Default Re: Noob

It can be done, I have seen it advertised before. You would need a blaster, generator, oven, powders, etc.... I dont think it is a good idea to have the blast booth double as a spray booth, too big of risk of contaminating parts.
Reply With Quote
  #3 (permalink)  
Old 10-13-2005, 12:42 AM
sdold's Avatar
Amateur Metal Finisher
 
Join Date: Jul 2005
Posts: 221
sdold is on a distinguished road
Default Re: Noob

It seems like it would need a lot of electricity if you used curing lamps, unless they could run on gas.
Reply With Quote
  #4 (permalink)  
Old 10-14-2005, 07:37 PM
Newbie
 
Join Date: Oct 2005
Posts: 2
c_hale007 is on a distinguished road
Default Re: Noob

Any suggestions?
Reply With Quote
  #5 (permalink)  
Old 10-14-2005, 08:23 PM
jimcarry's Avatar
Experienced Metal Finisher
 
Join Date: Jul 2004
Location: Arkansas
Posts: 370
jimcarry is on a distinguished road
Send a message via Yahoo to jimcarry
Default Re: Noob

If you are talking about Powder Coating I think your biggest problems would be powering your
shop what is your idea for this .
Then transport I would think possibly an old race car trailer so everything is inside what exactly
are your thoughts . I believe anything can be done if you want it bad enough
__________________
Jim Eaton
Reply With Quote
  #6 (permalink)  
Old 10-14-2005, 08:54 PM
mcaswell's Avatar
Caswell Inc Founder
 
Join Date: Nov 2001
Location: Lyons, NY USA
Posts: 2,357
Blog Entries: 1
mcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to behold
Default Re: Noob

This question crops up occasionally. Personally, I can never see the cash value or marketability of such a scheme. I doubt people are going to bring work to a mobile shop on a car show, and expect it to be done in a couple of hours.
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
I'm a noob trying to plate sheet metal USARMYnoob Electroplating Questions 1 08-03-2005 09:34 PM
Sand or bead blasting Q sorry, im a noob just starting Paintbalaguy Other Metal Finishing Questions 3 07-19-2005 09:20 AM
Questions about masking and plugging and rectifiers, noob Paintbalaguy Anodizing Questions 5 07-18-2005 08:28 PM
Noob ? about cure temps jsyi Powder Coating Questions 3 07-01-2004 01:37 AM
noob questions Scottbot Electroplating Questions 0 05-09-2004 07:07 PM


All times are GMT -4. The time now is 11:31 PM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.