Default What to do?

Guys, I'm in a quandry! I have a customers rim (black) that was damaged by some stained **** in somewhat white. I got it off with something stronger than alcohol, but I want to touch up the rim without messing it up thus having to strip and start over. Is there a polish that I can use to buff it shiny again?
I don't know about the owner, but I can live with that especially if it's for free.
I still have to buy paint to redo his centercap. No more freebies...
Reply With Quote
  #2 (permalink)  
Old 10-27-2005, 11:20 PM
pickleboy's Avatar
Metal Finishing Guru
 
Join Date: Feb 2005
Location: belleville michigan
Posts: 635
pickleboy is just really nicepickleboy is just really nicepickleboy is just really nicepickleboy is just really nice
Default Re: What to do?

i personally have not done it but if the finish is powder and was done right it should be able to be buffed with superfine cut compound just like regular paint then wax and it should be ok.
__________________
when in doubt polish it out/ why replace it when you can refinish it
G2 Polishing and Powdercoating
Reply With Quote
  #3 (permalink)  
Old 10-27-2005, 11:32 PM
sswee's Avatar
Moderator
 
Join Date: Nov 2004
Location: close to Austin, Texas
Posts: 1,229
sswee is a jewel in the roughsswee is a jewel in the roughsswee is a jewel in the roughsswee is a jewel in the rough
Default Re: What to do?

Check where they sell auto paint. For blemishes in liquid I wet sand 2000 to clean, buff with a rubbing compound and finish off with a hand glaze.
Reply With Quote
  #4 (permalink)  
Old 10-28-2005, 04:32 PM
Amateur Metal Finisher
 
Join Date: Mar 2005
Posts: 64
Heavykote
Default Re: What to do?

You guys are right. Geeez I'm a dummy! I do spraypainting, but I don't do it very much. Back to work...Thanks
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off


All times are GMT -4. The time now is 08:57 AM.


Powered by vBulletin® Version 3.7.4
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0
Copyright © Caswell Inc.