Trying to get into a corner I wound up building enough powder to get a run on a set of handlebars. Can I just and down that area and throw it in the oven quick to smooth it out or do I need to respray? Its not a super important job so if I have to respray I'll just leave it as is but if I can make the run less noticable I'd love to. The sooner someone can the respond the better, I'd love to get this piece finished tonight.
Thanks, Adam |
|
|||
|
That worked pretty well. It not perfect but I didnt work at it very hard at all. It on the underside of handle bars so the finish isnt super important but if I had worked at it harder I'm sure I could have gotten them nearly flawless.
Thanks Adam |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| One quick question about PC heat durability | UnorthodoxCreations | Powder Coating Questions | 1 | 09-19-2005 01:07 AM |
| Quick question regarding which kit... | L98-Z | Electroplating Questions | 0 | 06-24-2004 04:40 AM |
| Quick question... wasn't sure where to post it. | TCalYen | Other Metal Finishing Questions | 0 | 04-26-2004 08:44 AM |
| Quick question about pricing. | berad001 | Metal Polishing Questions | 3 | 02-07-2004 12:14 AM |
| I'm a first time powder coater. I have a quick question | Silverlex02 | Powder Coating Questions | 8 | 09-14-2003 03:59 PM |