I bought some wrinkle red powder and cannot seem to really get the wrinkle I should be out of it. I have tried it 2 times. first time at 400 for 10 min's second time I tried it at 350 for 20 min's both times it came out looking like this. Anyone have any idea's of what I would be doing wrong?
![]()
|
|
|||
|
Once you know the part is actually to temp..."for sure". That's one of the problems with the smaller ovens, they heat up to quick and the part never see's the temp it needs.
I'd do 400 for 25 mins. You can see the thicker areas of the part is kind of shinny. IMHO |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Robin Red Wrinkle | Crimson | Powder Coating Questions | 0 | 11-08-2005 08:56 AM |
| wrinkle not wrinkling | jtagger19 | Powder Coating Questions | 6 | 10-06-2005 08:17 PM |
| Black Wrinkle | warchild | Powder Coating Questions | 4 | 03-18-2005 07:52 PM |
| Which HB Fuller Color is Robin Red Wrinkle? | Noob2PC | Powder Coating Questions | 2 | 04-22-2004 08:43 PM |
| Wrinkle finish | matrob | Powder Coating Questions | 7 | 07-22-2003 09:10 PM |