I am just getting into powder coating and was looking for some plans to build a spray booth. I did find some pics of booths others were using, but none with good instructions on what parts were used and of the construction. Any help would be great here, I'm looking to build a booth with circulation fans and such. Thanks,

Jason
Reply With Quote
  #2 (permalink)  
Old 12-29-2005, 01:12 PM
Experienced Metal Finisher
 
Join Date: Jun 2004
Posts: 346
Popeye is an unknown quantity at this point
Default Re: Spray Booth Plans?

Jason,
How big of a booth?
Reply With Quote
  #3 (permalink)  
Old 12-29-2005, 11:57 PM
Newbie
 
Join Date: Dec 2005
Posts: 11
Helf8704 is on a distinguished road
Default Re: Spray Booth Plans?

I would like to build something big enough for car wheels and such, so that I wouldn't have to replace it too quickly. I will mainly be coating small auto parts, so I'm willing to work with an oven top booth for now. Thanks,

Jason
Reply With Quote
  #4 (permalink)  
Old 10-23-2007, 08:58 PM
Newbie
 
Join Date: Sep 2007
Posts: 8
pappahenn is on a distinguished road
Default Re: Spray Booth Plans?

I am looking for a booth size 6 wide by 36-48" deep by 80 inched tall. Any ideas
Reply With Quote
  #5 (permalink)  
Old 10-24-2007, 03:35 AM
Metal Finishing Guru
 
Join Date: Jun 2006
Posts: 568
Banditperformance is on a distinguished road
Default Re: Spray Booth Plans?

I built my booth like a closet. 5'w, 5'd, 7't With an exhaust fan in the back of it. Works good. I have a bench piece I slide in to catch the waste powder. It's a piece of 5/8" MDF. Nice and smooth adn powder doesnt stick to it. I use it when I am doing large batches to catch the waste and I reclaim it. get 1 cup reclaim for every 3 cups sprayed. Sometimes I am spraying 7-10 pounds a day, so reclaim adds up fast
__________________
Dan Pesonen
Bandit Powder Coat <<From Powder to Perfection>>
Forest Grove, BC Canada

Personal motto:
"If it ain't broke, modify somethin till it is"
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
building a spray booth daveg Powder Coating Questions 12 12-28-2007 05:38 PM
spray booth sorta done Blademan Powder Coating Questions 3 04-21-2004 04:39 PM
Spray Booth size???? Noob2PC Powder Coating Questions 2 03-30-2004 10:26 AM
SPRAY BOOTH SHIVERS Powder Coating Questions 19 12-10-2003 02:35 PM
spray booth skeleton Powder Coating Questions 1 05-12-2003 03:31 PM


All times are GMT -4. The time now is 07:26 AM.


Powered by vBulletin® Version 3.7.0
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.