i am going to be applying the Physco Lime topcoat with a Super Chrome under coat to my friends dirtbike frame.As well as the Physco Yellow with gold flake with Super chrome under coat to another friends dirtbike frame.
I recall reading on the forumns awhile back about the process,but cant seem to find it. If i recall correctly.I need to preheat the frame then allow to cool to around 160 then apply my coat of super chrome.Flash bake for roughly 10 minutes then apply the candy coat.Also when do I need to add the flake,can I just mix it in the physco yellow or is it going to be a 3 step process? Can some one varify this and or go into a little more detail for me,oven temps and cook times for each coat.Thank you in advance.Eric Last edited by RockPunk; 01-26-2006 at 01:00 AM. |
|
|||
|
here how I do it
(I always mix the flakes with clear they look better) fully cure chrome and allow to cool pre heat the chrome to 150 shoot the candy color and patially cure for 10-15 minutes allow to cool to 150 and shoot the clear with flakes fully cure |
|
|||
|
I tried to hot shoot a candy color over chrome powder once. Turned out horrible. I no longer shoot anything hot. Always allow it to cool.. cames out looking great.
Full cure between each step. |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| candy candy candy looks hot! | 11111111 | Powder Coating Questions | 8 | 03-12-2005 02:26 AM |
| 3 coat process | tavo1765 | Powder Coating Questions | 2 | 03-10-2005 04:36 PM |
| Candy top coat cracked | ricelake | Powder Coating Questions | 4 | 02-19-2005 07:04 AM |
| candy color? | randygrapes218 | Powder Coating Questions | 1 | 01-03-2005 12:09 AM |
| Powder Coat caught on fire! | Sleepr_Tech | Powder Coating Questions | 3 | 09-10-2004 07:22 AM |