im worried when i take the block down and blast it, when i go to clean it with iron phospate and i go to dry it will it flash rust and the other problem of making shure all the sandblast media out of it any tips or tricks,thanks
im worried when i take the block down and blast it, when i go to clean it with iron phospate and i go to dry it will it flash rust and the other problem of making shure all the sandblast media out of it any tips or tricks,thanks
Take it to a machine shop and have it hot tanked. I paid $20 to have it done.
Ok here is how I do them:
1 Engine only comes to me after it has been to the machine shop
A: Degreased
B: Been worked on and ready for assy.
2. Bead blast block heads oil pan etc.
3. Spray with acetone from a bottle ( WEAR A MASK )
4. Let dry and powder coat..
Jim S...
Jim Shuster
www.backyardpowdercoating.com Sold.....
www.chrissys68mustang.com Hobbie
www.photogserver.net Web Hosting.
Same here. and if they insist I just go ahead and take it as is and charge extra My shop rate is $75/hr and people pay it.Originally Posted by hvac36