Default The most basic of 'clear' questions

I can't seem to find the difference between super clear and HFSD. Can someone enlighten me?
Reply With Quote
  #2 (permalink)  
Old 03-21-2006, 07:49 PM
lcaswell's Avatar
Caswell Inc President
 
Join Date: Jan 2001
Location: Lyons NY USA
Posts: 2,353
Blog Entries: 3
lcaswell has much to be proud oflcaswell has much to be proud oflcaswell has much to be proud oflcaswell has much to be proud oflcaswell has much to be proud oflcaswell has much to be proud oflcaswell has much to be proud oflcaswell has much to be proud of
Default Re: The most basic of 'clear' questions

The Super High Gloss clear has a slightly higher gloss rating.
__________________
--
Lance Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm

Please support the moderators on our site by leaving reputation for their helpful posts. Read more here.
Reply With Quote
  #3 (permalink)  
Old 04-06-2006, 08:31 PM
warchild's Avatar
Amateur Metal Finisher
 
Join Date: Feb 2003
Location: Seymour,Tn.
Posts: 147
warchild
Default Re: The most basic of 'clear' questions

I can only tell the diffrence when on chrome.
I sprayed super clear on one side of a part of real chrome and then used the HFSD clear on the other side,
The super clear has a little bit more gloss and it does look a little bit better on the super chrome powder. it don't dull it as much as the older clear
__________________
WARCHILD
Reply With Quote
  #4 (permalink)  
Old 04-06-2006, 10:48 PM
machone's Avatar
Amateur Metal Finisher
 
Join Date: Jun 2005
Location: White Lake Michigan
Posts: 93
machone will become famous soon enough
Default Re: The most basic of 'clear' questions

There's gloss percentage listed in the Caswell catalog right along with the prices. Don't know if it's on the site
mach
__________________
TSA Custom Metal Finishes
Live fast, Die sideways
Reply With Quote
  #5 (permalink)  
Old 04-06-2006, 11:36 PM
sswee's Avatar
Moderator
 
Join Date: Nov 2004
Location: close to Austin, Texas
Posts: 1,212
sswee is a jewel in the roughsswee is a jewel in the roughsswee is a jewel in the roughsswee is a jewel in the rough
Default Re: The most basic of 'clear' questions

It was on the site on the details pop up.
SS
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
clear coating polished alum hybred Metal Polishing Questions 7 08-08-2005 02:58 PM
Fumes and basic newbie questions PeterBusch Anodizing Questions 7 10-05-2003 09:30 PM
Basic anodize questions erogers Anodizing Questions 0 03-12-2003 07:54 PM
A few polishing questions scimitartoo Metal Polishing Questions 1 02-10-2003 02:34 PM
Clear coating? Derrick Metal Polishing Questions 9 06-16-2002 10:34 PM


All times are GMT -4. The time now is 11:46 AM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.