ok fellows powder coater one time for all i want know
CAN YOU POWDER COAT HEADER WITH REGULAR POWDER some people told me it was done before whit good results friday i gonna have to pc smoke chrome over chrome on a muffler (vance and hine, is it the good spelling dohh)) and the protector part over the exhaust pipe the protector part d ont touch the exhaust pipe so i guess no problemo but for the muffler im not sure youre knowledge welcome |
|
|||
|
I can garante it won't work
I tried many times it will bubble up and peel off in fact high temp powder is the only one that I have had good results with and not for a long time normal temp on a harley bike is 600-700 riding it's higger only ceramic coat will work I've done heat covers with no problems |
|
|||
|
i did the job yesterday
i did the heat shield protector black smoke and the muffler whit black velvet high temp the customer was very happy whit the look that give. for the head pipe ,i did not pc it we decide to leave it chrome thank for the infos you saved me a lot of problems |
|
|||
|
the customer came back yesterday whit the pipe
the pc on the heat protector was completely burn and peel off the pipe and the muffler bottom part look like it was muffler the people at the bike shop did not leave an air gap between the pipe and the heat shield ? for the muffler i guess shooting right over chrome was not a good ideathe customer was in a good mood believe me so i sandblasted all the parts and sand it whit 180 grit sand paper and shoot it high temp flat black asking him to make sure to leave an air gap between the part and build a custom protector for the bottom of the slip on something like this ever happened to you, what you think gonna happen next |
|
|||
|
sorry for the mistake about (the pipe and the muffler bottom part look like it was muffler ) a real nobel price doooh
what i mean the bottom part of the muffler looked like it was sandblasted sorry if i scaped some of youre brain cell,it happen when you translate french to english ,eating and thinking at the next job at the same time |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| info on blast media | Blademan | Powder Coating Questions | 7 | 05-18-2007 06:58 PM |
| I think I'm gonna try greaseless! But I need some info | rides20 | Metal Polishing Questions | 7 | 07-19-2005 09:59 AM |
| PnP Nickel kit info needed. | remotestartdepot | Electroplating Questions | 1 | 01-08-2005 07:08 PM |
| Product info and Tecnique options | r2nailer | Metal Polishing Questions | 3 | 01-07-2004 03:17 AM |
| powder info | drfjr1976 | Powder Coating Questions | 6 | 12-30-2003 10:53 AM |