| Notices |
| Powder Coating Questions Discussion Board For powder coating questions. |
![]() |
|
|
Thread Tools | Display Modes |
|
|||
|
I am still having a problem with cast aluminum, such as intake manifolds. I am getting black dots impregnated into the aluminum that are showing quite vividly after PC'ing. I use 80g alum oxide, my air is super dry and clean. Please help.
Thanks in advance, Deke |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Something for you die hard polishers out there to chew on | thesound | Metal Polishing Questions | 15 | 12-03-2007 12:16 PM |
| Problems w/ cast aluminum | sthomag | Metal Polishing Questions | 2 | 02-03-2006 01:41 AM |
| Polishing cast aluminum | turbohardtop | Metal Polishing Questions | 26 | 07-05-2005 10:10 AM |
| Cast Aluminum | scocklin | Anodizing Questions | 5 | 12-03-2004 11:38 PM |
| Cast Aluminum HELP !! | JHFGSX9D | Metal Polishing Questions | 7 | 01-11-2004 01:22 AM |