  #1 (permalink)  
Old 04-11-2006, 09:30 PM
Newbie
 
Join Date: Mar 2006
Posts: 7
dekebell is on a distinguished road
Default Cleaning aluminum

What degreasers are you guys using to clean cast aluminum parts of oil? Anyone using a tank in the bigger shops that can advise on which chemicals and process to use?

Thanks,
Deke
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
I found sand blasting aluminum prior to powder coating is a big no-no. mtumbleson Powder Coating Questions 59 04-07-2008 07:37 PM
Something for you die hard polishers out there to chew on thesound Metal Polishing Questions 15 12-03-2007 12:16 PM
using aluminum as a cathode scocklin Anodizing Questions 19 03-31-2007 12:18 AM
cleaning anodized aluminum rancidnsx Anodizing Questions 0 01-26-2005 11:56 PM
Cleaning Oxidized Aluminum With Sand Blasting Media? freematt Other Metal Finishing Questions 2 02-23-2004 02:22 AM


All times are GMT -4. The time now is 03:09 PM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.