Thread: Can you figure out what I did wrong?

  1. #11

    Default Re: Can you figure out what I did wrong?

    If I am doing a two coat process I usually pull right out of the oven and apply second coat without cleaning with any chemicals just blow of with blow gun this works much better sometimes chemicals cause odd reactions . If the product recieves first coat and sits for a while or is handled alot I clean with denatured alcohol and preheat this has cured most problems.
    http://home.earthlink.net/~custompowdercoating/
    http://www.nccustomcoating.com
    North carolina powder coating custom powder coating motorcyle powder coating hot rod powder coating candy chrome powder coating powder coating powder coating powder coating powder coating powder coating powder coating powder coating powder coating
    Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
    Reply With Quote Reply With Quote  
    Share with Facebook

  2. #12
    Join Date
    Mar 2005
    Posts
    200

    Default Re: Can you figure out what I did wrong?

    Quote Originally Posted by 3000gtvr4
    I have had some issuses with The chrome. I think the chrome dosnt like to cure more than once.
    Your kidding right?
    Thats all I use the chrome powders for... basecoats to put the candy colors over the top of.

    And I never touch it anymore than I HAVE to inbetween coats.
    Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
    Reply With Quote Reply With Quote  
    Share with Facebook

+ Reply to Thread
Page 2 of 2
FirstFirst 1 2

Thread Information

Users Browsing this Thread

There are currently 1 users browsing this thread. (0 members and 1 guests)

     

Similar Threads

  1. Cartridge rolls - description wrong?
    By mpierich in forum Caswell Please Sell This...
    Replies: 1
    Last Post: 06-14-2005, 11:52 PM
  2. Ok,what am I doing wrong
    By mach1man in forum Metal Polishing Questions
    Replies: 1
    Last Post: 08-18-2004, 07:31 PM
  3. cant figure out the chrome
    By Carcher7878 in forum Powder Coating Questions
    Replies: 2
    Last Post: 05-21-2004, 01:05 PM
  4. What's wrong here......
    By dsacco1013 in forum Powder Coating Questions
    Replies: 2
    Last Post: 01-05-2004, 10:15 PM
  5. What am I doing wrong here
    By PC101 in forum Powder Coating Questions
    Replies: 3
    Last Post: 06-29-2003, 10:14 PM

Bookmarks

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts

Search Engine Friendly URLs by vBSEO 3.5.0 RC1 PL1