  #1 (permalink)  
Old 06-19-2006, 08:57 PM
baz baz is offline
Experienced Metal Finisher
 
Join Date: Feb 2006
Posts: 349
baz has a spectacular aura aboutbaz has a spectacular aura about
Default wrinkle black

i am looking for a texture black to match harley engine cases i need something finer then caswell s black wrinkle , any suggestions ? thanks ,
i know columbia has a black fine texture but last time i placed an order with them .took more than 2 weeks to get to canada .c ant wait that long
Reply With Quote
  #2 (permalink)  
Old 06-20-2006, 07:43 AM
Amateur Metal Finisher
 
Join Date: Jul 2005
Posts: 88
Crimson
Default Re: wrinkle black

like this wrinkle black?



Reply With Quote
  #3 (permalink)  
Old 06-20-2006, 06:58 PM
Amateur Metal Finisher
 
Join Date: Mar 2006
Location: Ohio
Posts: 94
FSTFBDY is on a distinguished road
Default Re: wrinkle black

I use a Dupont BW
http://www.cecoatings.com/images/coa...s/DSC02410.JPG
http://www.cecoatings.com/images/coa...vavlecover.jpg
http://www.cecoatings.com/images/coa...on%20Elbow.jpg

Last edited by FSTFBDY; 06-20-2006 at 07:02 PM.
Reply With Quote
  #4 (permalink)  
Old 06-20-2006, 10:55 PM
baz baz is offline
Experienced Metal Finisher
 
Join Date: Feb 2006
Posts: 349
baz has a spectacular aura aboutbaz has a spectacular aura about
Default Re: wrinkle black

thanks guys , the dupont looks a bit too coarse for what i need .crimson's pictures look a bit finer but i m not sure,it s hard to judge a texture from a picture,
crimson wich paint is it anyway . thanks again for taking the time for me guys
Reply With Quote
  #5 (permalink)  
Old 06-21-2006, 08:58 AM
Amateur Metal Finisher
 
Join Date: Jul 2005
Posts: 88
Crimson
Default Re: wrinkle black

FSTFBDY have you ever used the wrinkle red from DuPont? I am trying to find a red to use on Honda valve Covers for that JDM look. Have not had any luck finding a powder that works the way I want.
Reply With Quote
  #6 (permalink)  
Old 06-21-2006, 04:19 PM
Amateur Metal Finisher
 
Join Date: Mar 2006
Location: Ohio
Posts: 94
FSTFBDY is on a distinguished road
Default Re: wrinkle black

sorry no I havent.
Reply With Quote
  #7 (permalink)  
Old 07-17-2006, 03:50 PM
Amateur Metal Finisher
 
Join Date: Mar 2005
Posts: 202
mtnbiker is an unknown quantity at this point
Default Re: wrinkle black

Hmmm... Caswell wrinkle was pretty close to the Nightrain cover I did.
Reply With Quote
  #8 (permalink)  
Old 08-14-2007, 06:41 PM
Amateur Metal Finisher
 
Join Date: Feb 2007
Posts: 64
hbracing is on a distinguished road
Default Re: wrinkle black

where do you get the Dupont powder? I have been to the dupont site and its not very helpful or maybe and could be I am a little computer challenged which I will admit.............
Reply With Quote
  #9 (permalink)  
Old 08-14-2007, 07:43 PM
Harleydad's Avatar
Metal Finishing Guru
 
Join Date: Dec 2006
Location: Wisconsin
Posts: 573
Harleydad is an unknown quantity at this point
Default Re: wrinkle black

Quote:
Originally Posted by baz View Post
i am looking for a texture black to match harley engine cases i need something finer then caswell s black wrinkle , any suggestions ? thanks ,
i know columbia has a black fine texture but last time i placed an order with them .took more than 2 weeks to get to canada .c ant wait that long
Have you tried Tiger Drylac? They have black wrinkle, black texture and a black fine texture.
Reply With Quote
  #10 (permalink)  
Old 08-14-2007, 09:02 PM
Metal Finishing Guru
 
Join Date: Jun 2006
Posts: 613
Banditperformance is on a distinguished road
Default Re: wrinkle black

Quote:
Originally Posted by hbracing View Post
where do you get the Dupont powder? I have been to the dupont site and its not very helpful or maybe and could be I am a little computer challenged which I will admit.............
I get mine form Cloverdale paints
__________________
Dan Pesonen
Bandit Powder Coat <<From Powder to Perfection>>
Forest Grove, BC Canada

Personal motto:
"If it ain't broke, modify somethin till it is"
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Super mirror black or low gloss black? Deecoat Powder Coating Questions 2 03-09-2006 10:24 PM
After 1500g sanding, and black emery, frame has black streak fizlfry Metal Polishing Questions 8 04-26-2005 10:09 AM
Caswell burner black? mtnbiker Powder Coating Questions 1 04-13-2005 12:15 PM
Black Wrinkle warchild Powder Coating Questions 4 03-18-2005 06:52 PM
White Compound Turns Black? GrillMan Other Metal Finishing Questions 2 08-23-2003 02:12 AM


All times are GMT -4. The time now is 02:43 AM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.