Default powder types

The Caswell catalog does not mention the powder types it sells. Are your powders epoxy,epoxy-polyester hybrid, urethane, tgic polyester,silicone-polyester? It would make it easier to purchase from you if I had a list of which is which in your catalog.
Reply With Quote
  #2 (permalink)  
Old 01-20-2003, 01:08 PM
mcaswell's Avatar
Caswell Inc Founder
 
Join Date: Nov 2001
Location: Lyons, NY USA
Posts: 2,357
Blog Entries: 1
mcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to behold
Default

This info will be on the new web site when it launches:

All powders are TGIC except the Flat Black, which is Epoxy and the White, which is an epoxy hybrid.
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Reply With Quote
  #3 (permalink)  
Old 01-20-2003, 09:22 PM
Experienced Metal Finisher
 
Join Date: Dec 2002
Location: Central New York
Posts: 353
DALE will become famous soon enough
Default caswell

Thank you.
Reply With Quote
  #4 (permalink)  
Old 01-20-2003, 11:07 PM
Amateur Metal Finisher
 
Join Date: Aug 2002
Location: Mississippi Gulf Coast
Posts: 133
marsfrogie
Send a message via AIM to marsfrogie
Default

Are the epoxy based powders prone to chalking after a few years?
Reply With Quote
  #5 (permalink)  
Old 01-29-2003, 10:32 PM
Experienced Metal Finisher
 
Join Date: Dec 2002
Location: Central New York
Posts: 353
DALE will become famous soon enough
Default

I haven't noticed any but you must match the powder to the application.Use the TGIC if it's for exterior use, otherwise the epoxy is very good powder.
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Tips and Tricks non-stick Powder Coating Questions 27 11-11-2007 03:01 PM
Finding a place to powder coat RCLSolutions Powder Coating Questions 3 05-04-2005 10:42 PM
Gun spitting excess powder pdeinc Powder Coating Questions 8 10-21-2004 04:21 PM
Can I mix types of powder? Hemi-T Powder Coating Questions 6 04-18-2003 11:56 PM
Types of material that can be powder coated. bryaneh Powder Coating Questions 1 03-03-2003 08:31 PM


All times are GMT -4. The time now is 04:48 PM.


Powered by vBulletin® Version 3.7.4
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0
Copyright © Caswell Inc.