Default Super Wet Black easily scuffed

I have been getting better at PCing parts and have been getting good finishes, mostly. I have noticed that the Super Wet Black coated parts are easily scuffed. If there is any dust on the part and I brush it off with my finger, the surface will have light scratches or scuffs on it. Are the parts not fully cured (either under or over cured) or is that the nature of the Super Wet Black?
Reply With Quote
  #2 (permalink)  
Old 09-24-2006, 04:45 PM
Newbie
 
Join Date: Mar 2005
Posts: 16
KeithLambert7
Default Re: Super Wet Black easily scuffed

That's been my experience as well. I think its just the nature of the finish. I've never has any returns, but I've noticed it. People seem to love it. I recommend that it be waxed to protect from this problem.
Reply With Quote
  #3 (permalink)  
Old 10-03-2006, 09:31 AM
Amateur Metal Finisher
 
Join Date: Mar 2005
Posts: 202
mtnbiker is an unknown quantity at this point
Default Re: Super Wet Black easily scuffed

Yup... the more glossy the powder... the more likely of these fine scratches.
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Super mirror black or low gloss black? Deecoat Powder Coating Questions 2 03-09-2006 11:24 PM
Super wet black question petshe25 Powder Coating Questions 3 03-03-2006 05:17 PM
White Compound Turns Black? GrillMan Other Metal Finishing Questions 2 08-23-2003 03:12 AM


All times are GMT -4. The time now is 04:54 PM.


Powered by vBulletin® Version 3.7.4
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0
Copyright © Caswell Inc.