hey peoplezz..been awhile..found this neat little trick this summer working on my vette...this will degrease and strip paint and even powder coated stuff...depending upon the size part....i used an old metal barrel...good old crystal drano....not the liquid...just mix with some water and let errr soak..i agitated mine with one of those long paint mixer rods that fit on a drill.sure cleaned up the parts sweet...just for laughs i dropped in some stuff i had pc and the powder peeled right off...dont remember how long it took...but it was faster than blasting...
__________________
Pro-Tech Powder Coating 93976 Ocean Way 541-247-8168 protech@harborside.com Gold Beach,Oregon |
|
|||
|
you can also remove anodize with crystal drano , be very careful with that .another word for that stuff is caustic soda or sodium hyroxyde, if properly diluted could be used for etching aluminium parts , if not properly mixed you could damage or completely destroy aluminium parts ,believe me i know
|
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Stripper... | KZjim | Powder Coating Questions | 9 | 07-03-2005 10:15 AM |
| Stripper? | 00_buckshot | Anodizing Questions | 4 | 01-27-2004 06:38 PM |
| Anodizing Stripper | Tim Wiltse | Anodizing Questions | 3 | 09-26-2003 12:12 PM |
| annodize stripper | saiyan7 | Metal Polishing Questions | 2 | 12-05-2002 11:29 AM |
| anodizing stripper | rrdble | Metal Polishing Questions | 1 | 10-14-2002 10:22 AM |