Default multiple layers

I powder coated a part and I found an area that I must of scraped when it was still hot and now I have to fix it. I would rather not stripe it if I can avoid it. I used red sparkle and clear. my question is can I shoot another coat of red and clear or will this be a problem?
__________________
Rich
project 1
http://www.freewebs.com/boston_jake01/index.htm
Reply With Quote
  #2 (permalink)  
Old 12-18-2006, 10:18 PM
Experienced Metal Finisher
 
Join Date: Apr 2004
Posts: 466
jtagger19 is on a distinguished road
Default Re: multiple layers

you can but you shouldn't
I never re coat after clear or a 3rd coat ( candys and clear)
it might be a problem in a few months like peeling .

but if you feel like it won't mater to you , you can blast it at 30PSI with 80-120 grit or use a 220 sandpaper and re coat
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Curing multiple parts? j-mcguigan Powder Coating Questions 1 04-21-2004 07:59 AM
Curing multiple parts of varying size in oven at same time?? Fireblade Powder Coating Questions 3 09-28-2003 09:10 AM
Gold Plating multiple items at once jonramos Electroplating Questions 2 09-05-2003 10:54 PM
Problems with clear, flowout, multiple colors, more... allcarfan Powder Coating Questions 3 08-25-2003 10:49 PM
anodizing with multiple colors july_favre Electroplating Questions 1 01-08-2003 06:39 PM


All times are GMT -4. The time now is 05:27 PM.


Powered by vBulletin® Version 3.7.4
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0
Copyright © Caswell Inc.