Default looking for a bright orange

is the pumpkin a bright orange? I want something bright, almost neon-orange!


thanks,

nutty
Reply With Quote
  #32 (permalink)  
Old 11-16-2003, 09:09 PM
Amateur Metal Finisher
 
Join Date: Mar 2003
Location: S. IL.
Posts: 109
drfjr1976
Default

How about more Transparents/top coats/ tinted clears. I am looking for some of this color (picture below) It is called "lollypop Blue". Its a deep blue with a hint of purple.
Reply With Quote
  #33 (permalink)  
Old 11-16-2003, 10:07 PM
Experienced Metal Finisher
 
Join Date: Sep 2003
Location: CT-NY-NJ area
Posts: 359
non-stick
Default

Duly noted and it shall be "sought after" for you. I have it on good authority that there will be a "color explosion" happening here soon with lots of other little goodies thrown into the mix..... Russ
Reply With Quote
  #34 (permalink)  
Old 12-15-2003, 01:58 PM
Experienced Metal Finisher
 
Join Date: Sep 2003
Location: CT-NY-NJ area
Posts: 359
non-stick
Default

high-gloss clear might spice things up around here.
Reply With Quote
  #35 (permalink)  
Old 12-28-2003, 09:31 PM
Experienced Metal Finisher
 
Join Date: Dec 2002
Location: Central New York
Posts: 353
DALE will become famous soon enough
Default

How about adding HB Fuller's Midnight blue?
Reply With Quote
  #36 (permalink)  
Old 01-14-2004, 11:29 AM
Newbie
 
Join Date: Jan 2004
Posts: 4
LiquidDreamLAD
Default

The only thing I see you guys missing is a really nice bronze color something like this http://www.nissanperformance.net/nismo/bronze_alloy.jpg
its a pretty hard to find color and also pretty friggin popular, trust me
Reply With Quote
  #37 (permalink)  
Old 02-08-2004, 02:18 PM
Newbie
 
Join Date: Oct 2003
Posts: 2
93BlackFD
Default

harley orange

any recommendations?
Reply With Quote
  #38 (permalink)  
Old 03-25-2004, 08:19 PM
Amateur Metal Finisher
 
Join Date: Jan 2004
Location: Beaufort, SC
Posts: 121
WAORacing
Default

This is something that everyone would like to see i think.
7" x 11" Hi-Temp Masking Sheets 7/pack
I took some of these to a local sign shop and they were able to cut me out perfect lettering stencils.
Caswell do you think you will be able to get these?
Reply With Quote
  #39 (permalink)  
Old 04-22-2004, 04:38 AM
Newbie
 
Join Date: Apr 2004
Location: Findlay ohio
Posts: 42
Carcher7878
Send a message via AIM to Carcher7878 Send a message via Yahoo to Carcher7878
Default

how about a stand for people that use IR propane. Some people have heaters that just want the stand. Maybe go with the IR propane heat aswell with the electric. Also, have a book made up with how-to's oven builds, what nots. Your powder selection is great! I just need tools. lol

back to the HF. lol

Archer
Reply With Quote
  #40 (permalink)  
Old 05-14-2004, 09:59 AM
Newbie
 
Join Date: May 2004
Posts: 5
strongtower
Default

true florescents - not Safety Red, Orange, Yellow, etc.

and another "aye" for the tinted clears

p.s. got my Powderstore Caliber color chips. it says that they have the HB Fuller "complete range of powder products". do you know then if HBF has florescents?
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off


All times are GMT -4. The time now is 04:59 PM.


Powered by vBulletin® Version 3.7.4
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0
Copyright © Caswell Inc.