  #1 (permalink)  
Old 05-04-2007, 03:19 PM
Amateur Metal Finisher
 
Join Date: Aug 2005
Posts: 65
JeffL
Default Clear coat????

when using colors that require a clear top coat, can the clear be put on maybe a day or so after the base coat is shot?
Reply With Quote
  #2 (permalink)  
Old 05-04-2007, 06:27 PM
Metal Finishing Guru
 
Join Date: Jun 2006
Posts: 613
Banditperformance is on a distinguished road
Default Re: Clear coat????

Sometimes, but the sooner the better, especially for Chrome like powders
__________________
Dan Pesonen
Bandit Powder Coat <<From Powder to Perfection>>
Forest Grove, BC Canada

Personal motto:
"If it ain't broke, modify somethin till it is"
Reply With Quote
  #3 (permalink)  
Old 05-04-2007, 07:39 PM
nuttyman's Avatar
Metal Finishing Guru
 
Join Date: Sep 2003
Location: Rio Rancho, NM
Posts: 553
nuttyman
Default Re: Clear coat????

you'll have the best results if you shoot when the part is still hot.
__________________
SouthWest Powderworx
Tyler Nutter
5054803934
www.swpowder.com
myspace/swpowder
tyler@swpowder.com
Reply With Quote
  #4 (permalink)  
Old 05-05-2007, 06:37 AM
JTW37's Avatar
Metal Finishing Guru
Caswell Platinum Member
 
Join Date: Feb 2006
Location: Bristol, In
Posts: 514
JTW37 is an unknown quantity at this point
Default Re: Clear coat????

But be careful you don't overload it with clear. It's hard to tell how much your putting on when it is hot. But it's pretty cool to see it happen
__________________
Who says you can't teach an ole dog new tricks?
Reply With Quote
  #5 (permalink)  
Old 05-05-2007, 12:57 PM
Amateur Metal Finisher
 
Join Date: Aug 2005
Posts: 65
JeffL
Default Re: Clear coat????

What do you do if you shot say like 6 pieces?Do you do all in the base coat first, or do you clean out the gun & shot each piece in clear?
Reply With Quote
  #6 (permalink)  
Old 05-05-2007, 02:57 PM
nuttyman's Avatar
Metal Finishing Guru
 
Join Date: Sep 2003
Location: Rio Rancho, NM
Posts: 553
nuttyman
Default Re: Clear coat????

I have seperate guns. I always have a clear in 1 gun when doing 2 stage coats, & whatever is in the oven that needs a clear gets it all @ the same time.
__________________
SouthWest Powderworx
Tyler Nutter
5054803934
www.swpowder.com
myspace/swpowder
tyler@swpowder.com
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Extreme Chrome with Clear Coat How to... hvac36 Powder Coating Questions 47 02-06-2008 09:57 PM
Shiniest Chrome Powder, and do i need to clear coat it? investinwaffles Powder Coating Questions 5 07-20-2006 07:24 PM
cleaning brass before clear coat. ovrundr Metal Polishing Questions 5 08-31-2005 12:45 AM
Clear coat problem sportster883r Powder Coating Questions 3 11-21-2004 04:52 PM
reason for clear coat? Jay87T Powder Coating Questions 14 03-20-2004 11:41 AM


All times are GMT -4. The time now is 01:42 PM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.