Question Cure Process Temp ?

say my oven is up to 400deg, and my powder says 400deg for 20 minutes.

does that start when i put the part in or when the part itself comes up to 400deg using a laser temp guage?
Reply With Quote
  #2 (permalink)  
Old 06-20-2007, 08:36 PM
nuttyman's Avatar
Metal Finishing Guru
 
Join Date: Sep 2003
Location: Rio Rancho, NM
Posts: 553
nuttyman
Default Re: Cure Process Temp ?

when the part reaches temp. the powder will start to flow before it reaches temp keep in mind.
__________________
SouthWest Powderworx
Tyler Nutter
5054803934
www.swpowder.com
myspace/swpowder
tyler@swpowder.com
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
cure time and temp kmajka01 Powder Coating Questions 22 12-03-2007 01:13 AM
Oven temp vs part temp getastro Powder Coating Questions 4 10-01-2007 01:53 AM
Improving Plating Performance jimcarry Electroplating Questions 0 09-28-2005 09:50 AM
3 coat process tavo1765 Powder Coating Questions 2 03-10-2005 04:36 PM
Powder coating process.. tomg552001 Powder Coating Questions 4 01-14-2003 08:42 PM


All times are GMT -4. The time now is 05:37 PM.


Powered by vBulletin® Version 3.7.4
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0
Copyright © Caswell Inc.