Hi i run a small powder coating buisness in Australia and i always get asked if i can powder coat fibre glass and plastic for cars and some motor bikes. I am aware that i would need powder coat that would fully cure at lower temperatures but i was wondering if there is such a thing
![]() Any help would be great. |
|
||||
|
Quote:
Ditto on the UV coatings. |
|
||||
|
Quote:
Thanks for clarifying that! UV coatings are very limited in color and finish selection at this time. Jason |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| *** WE ARE GIVING AWAY FREE POWDER COATING *** | mcaswell | Powder Coating Questions | 197 | 07-08-2008 12:31 PM |
| I found sand blasting aluminum prior to powder coating is a big no-no. | mtumbleson | Powder Coating Questions | 59 | 04-07-2008 07:37 PM |
| powder coating over powder coat? | corybarta | Powder Coating Questions | 6 | 08-21-2006 08:15 AM |
| Fs: Turnkey Powder Coating And Ceramic Coating Business!!!! | Mcurtis7 | Used Items For Sale | 0 | 10-02-2005 02:18 PM |
| Non-paint powder coating | dshepherd | Powder Coating Questions | 6 | 01-26-2004 11:49 AM |