Question Translucent (Lollipop Red) Problem

This was my first time spraying a translucent over chrome.. Had some runs on several pieces. Seemed like maybe to much powder
Reply With Quote
  #2 (permalink)  
Old 07-29-2007, 05:38 PM
Harleydad's Avatar
Metal Finishing Guru
 
Join Date: Dec 2006
Location: Wisconsin
Posts: 573
Harleydad is an unknown quantity at this point
Default Re: Translucent (Lollipop Red) Problem

Quote:
Originally Posted by donafams
This was my first time spraying a translucent over chrome.. Had some runs on several pieces. Seemed like maybe to much powder
Yes, too much powder will cause you to get the runs.
Did you spray the part hot or cold?
Reply With Quote
  #3 (permalink)  
Old 07-29-2007, 07:15 PM
Metal Finishing Guru
 
Join Date: Jun 2006
Posts: 613
Banditperformance is on a distinguished road
Default Re: Translucent (Lollipop Red) Problem

I allways spray Lolly's Hot. Best way to ensure even coverage IMO
__________________
Dan Pesonen
Bandit Powder Coat <<From Powder to Perfection>>
Forest Grove, BC Canada

Personal motto:
"If it ain't broke, modify somethin till it is"
Reply With Quote
  #4 (permalink)  
Old 07-29-2007, 07:38 PM
nuttyman's Avatar
Metal Finishing Guru
 
Join Date: Sep 2003
Location: Rio Rancho, NM
Posts: 553
nuttyman
Default Re: Translucent (Lollipop Red) Problem

yup!!!! that'll happen. you have to get the hang of the candies to get good results.





__________________
SouthWest Powderworx
Tyler Nutter
5054803934
www.swpowder.com
myspace/swpowder
tyler@swpowder.com
Reply With Quote
  #5 (permalink)  
Old 07-29-2007, 08:42 PM
Amateur Metal Finisher
 
Join Date: Apr 2007
Posts: 229
donafams is on a distinguished road
Default Re: Translucent (Lollipop Red) Problem

well i ran it up to 400, pulled it out then sprayed it, but i think i out on more than i should because i had to shake the gun alot to get it to flow...my bad
Reply With Quote
  #6 (permalink)  
Old 08-01-2007, 07:28 AM
JTW37's Avatar
Metal Finishing Guru
Caswell Platinum Member
 
Join Date: Feb 2006
Location: Bristol, In
Posts: 551
JTW37 is an unknown quantity at this point
Default Re: Translucent (Lollipop Red) Problem

I've used green and blue, but did it cold. came out pretty good. Get the powder to look fuzzy, but not furry. It worked for me.
__________________
Who says you can't teach an ole dog new tricks?
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
transparent red powder over aluminum diamond plate controlsengineer Powder Coating Questions 2 02-01-2007 12:19 PM
mirror red q's krymis Powder Coating Questions 5 05-21-2006 11:04 PM
Candy red top coat mikekozura Powder Coating Questions 3 02-11-2006 10:59 PM
Anybody have a pic of translucent red? gtabadboy Powder Coating Questions 3 10-11-2005 10:43 PM


All times are GMT -4. The time now is 05:49 PM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.