Default C***!

Need some help. Just tried it today. When I start to spray, a **** load of powder falls out all at once. Two sec later it comes out real nice then a **** load of powder falls out all over my peice. Is my gun bad? I screwed in the nozel and it still happens. Any help?
Reply With Quote
  #2 (permalink)  
Old 08-03-2007, 11:16 PM
Metal Finishing Guru
 
Join Date: Jun 2006
Posts: 613
Banditperformance is on a distinguished road
Default Re: C***!

To much powder in cup will cause Burps like that
__________________
Dan Pesonen
Bandit Powder Coat <<From Powder to Perfection>>
Forest Grove, BC Canada

Personal motto:
"If it ain't broke, modify somethin till it is"
Reply With Quote
  #3 (permalink)  
Old 08-04-2007, 12:00 AM
Newbie
 
Join Date: Aug 2006
Posts: 46
zoeconner is on a distinguished road
Default Re: C***!

Thanks that was it. I thought is said at least 3 " of powder. I just filled the cup lol. Turned out great. Man it is really easy after that. Now back to more practice.
Reply With Quote
  #4 (permalink)  
Old 08-04-2007, 12:19 AM
Newbie
 
Join Date: Aug 2006
Posts: 46
zoeconner is on a distinguished road
Default Re: C***!

Im doing some Lollypop Blue but it comes out pretty dark. Do you have to do a white under it first or is it just best on allum? Ill try to post some pics
Reply With Quote
  #5 (permalink)  
Old 08-04-2007, 12:25 AM
Metal Finishing Guru
 
Join Date: Jun 2006
Posts: 613
Banditperformance is on a distinguished road
Default Re: C***!

Lolly powders are best on Shiny surfaces, Alum, or Chrome. They are a transparent clearcoat. So, they will let whatever base color shine through.
__________________
Dan Pesonen
Bandit Powder Coat <<From Powder to Perfection>>
Forest Grove, BC Canada

Personal motto:
"If it ain't broke, modify somethin till it is"
Reply With Quote
  #6 (permalink)  
Old 08-04-2007, 06:40 AM
Harleydad's Avatar
Metal Finishing Guru
 
Join Date: Dec 2006
Location: Wisconsin
Posts: 573
Harleydad is an unknown quantity at this point
Default Re: C***!

Adding to Bandits comments, the higher the film build the darker the color. Try less powder.
Reply With Quote
  #7 (permalink)  
Old 08-04-2007, 10:13 AM
Newbie
 
Join Date: Aug 2006
Posts: 46
zoeconner is on a distinguished road
Default Re: C***!

I was doing it on plane steel. Could that be why?
Reply With Quote
  #8 (permalink)  
Old 08-04-2007, 02:13 PM
nuttyman's Avatar
Metal Finishing Guru
 
Join Date: Sep 2003
Location: Rio Rancho, NM
Posts: 553
nuttyman
Default Re: C***!

yes of course. remember when working with transparent powders that the brighter the base the brighter the finish layer will be & obviously the same applies to a darker base.
__________________
SouthWest Powderworx
Tyler Nutter
5054803934
www.swpowder.com
myspace/swpowder
tyler@swpowder.com
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off


All times are GMT -4. The time now is 02:11 AM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.