I am using the power coat system to repaint some old erector set parts. I just got to try
out my new sprayer today very nice. Some of the pices came out different colors. I was using yellow couple of pices were real nice a couple came out like under spray. I though I had covered them about the same. My question is is my heat possibly inconsient or did I over bake? Another question can you apply to much power an cause the paint to run in the baking process? I have never been very good at painting but I think power coating is my answer to a good paint job for me. Thanks Amature Rick |
|
||||
|
Yes, you can apply too much powder and have it run.
We've forwarded the over baking question to our supplier and will let you know when we get an answer.
__________________
-- Mike Caswell Caswell Inc http://www.caswellplating.com Need Support? Visit our online support section at http://support.caswellplating.com Have A Web Site? Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Removal of unknown coating on aluminum | rclint | Metal Polishing Questions | 6 | 08-25-2005 12:04 AM |
| Coating Brake Rotors | rickanderson53 | Other Metal Finishing Questions | 4 | 08-18-2005 11:15 PM |
| Non-paint powder coating | dshepherd | Powder Coating Questions | 6 | 01-26-2004 11:49 AM |
| Anodizing Power Supply Q's | jnbsystems | Anodizing Questions | 7 | 10-02-2003 10:33 PM |
| Does a coating exist that can be bent slightly? | Augest | Powder Coating Questions | 1 | 09-22-2003 01:34 PM |