Newbie here, i searched and couldnt find any threads on how far a lb of pc goes.
I am going to paint my atv frame lolipop blue metallic, and need to know how much it takes. i use a lolipop blue base coat pluse a metalic clearcoat right? also, i couldnt find a High temp metallic blue OR red for brake calipers, will regular pc work on calipers w/out melting?? and im gong to be using a electric oven with the basic PC kit, how will i recycle the powder? thanks guys!! Last edited by pcer; 10-24-2007 at 06:55 PM. |
|
|||
|
Isnt lollipop blue a candy? If so then you have to coat your frame with a base color, like silver or gold, then apply the candy blue. The metallic from the base color will show thru, if you choose a metallic.
|
|
|||
|
For the atv frame i would have at least a 1/2 pound.It's always nice to have a little extra laying around.It also depends on the size of the frame.
For the brake calipers no just hi temp. powders are not nessary. |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| BMX Frame | fhmreader | Powder Coating Questions | 0 | 06-15-2006 06:57 PM |
| how much powder for motorycle frame? | tattoo72 | Powder Coating Questions | 2 | 02-18-2006 01:01 AM |
| powder coating a frame? | randygrapes218 | Powder Coating Questions | 5 | 06-25-2004 09:24 PM |
| How much powder for ATV frame | senna-the-great | Powder Coating Questions | 6 | 03-07-2004 08:48 PM |
| Gun Frame | warchild | Electroplating Questions | 1 | 06-06-2003 10:49 AM |