Plating Powder Coating Buffing Anodizing - Caswell Inc. Metal Finishing Forum  

Go Back   Plating Powder Coating Buffing Anodizing - Caswell Inc. Metal Finishing Forum > Powder Coating Questions

Notices

Powder Coating Questions Discussion Board For powder coating questions.

Reply
 
Thread Tools Display Modes
  #1 (permalink)  
Old 01-10-2008, 01:39 AM
Newbie
 
Join Date: May 2007
Posts: 35
jazzcornet is on a distinguished road
Default my first try!!!!

here are two pictures taken with a camera phone of a TB inlet off a 93 mr2t. first time ever powdercoating. my kit just came in today!! let me know what you think



Reply With Quote
  #2 (permalink)  
Old 01-10-2008, 05:54 AM
FigureLLC's Avatar
Experienced Metal Finisher
Caswell Platinum Member
 
Join Date: Nov 2005
Posts: 403
FigureLLC will become famous soon enough
Default Re: my first try!!!!

looks great! xtreme chrome with clear topcoat?
__________________
Len
Figure Engineering, LLC
Reply With Quote
  #3 (permalink)  
Old 01-10-2008, 01:00 PM
Newbie
 
Join Date: May 2007
Posts: 35
jazzcornet is on a distinguished road
Default Re: my first try!!!!

ironically enough, it's actually clear coat on the bottom with a xtreme chrome top coat!!! i wasn't paying attention to the can when i put it in my gun. but whatever, it was my first try and it was at 1130 at night
Reply With Quote
  #4 (permalink)  
Old 01-10-2008, 07:13 PM
Harleydad's Avatar
Metal Finishing Guru
 
Join Date: Dec 2006
Location: Wisconsin
Posts: 573
Harleydad is an unknown quantity at this point
Default Re: my first try!!!!

Ya better apply another coat of clear over the xtreme chrome.
Reply With Quote
  #5 (permalink)  
Old 01-10-2008, 08:09 PM
Newbie
 
Join Date: May 2007
Posts: 35
jazzcornet is on a distinguished road
Default Re: my first try!!!!

yeah, im thinking about it, but wont that dull it.
Reply With Quote
  #6 (permalink)  
Old 01-11-2008, 06:02 AM
FigureLLC's Avatar
Experienced Metal Finisher
Caswell Platinum Member
 
Join Date: Nov 2005
Posts: 403
FigureLLC will become famous soon enough
Default Re: my first try!!!!

oh! THAT explains why it looks so nice. yes, yes the clear will dull it. but it'll dull by itself without the clear top coat. nuttyman in another thread said the chrome looks best over gloss black.
__________________
Len
Figure Engineering, LLC
Reply With Quote
  #7 (permalink)  
Old 01-12-2008, 05:45 PM
Newbie
 
Join Date: Nov 2007
Posts: 40
jw450r1 is on a distinguished road
Default Re: my first try!!!!

any pics of this
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off


All times are GMT -4. The time now is 08:00 PM.