Just wondering if I could put clear powder coat over This

I want the same color, but this goes on in a very thin coat which isn't very durable.
Reply With Quote
  #2 (permalink)  
Old 02-11-2008, 08:26 PM
Experienced Metal Finisher
 
Join Date: Apr 2004
Posts: 466
jtagger19 is on a distinguished road
Default Re: PC over manifold paint

Exhaust Manifold or intake manifold ?
if it's for an exhaust manifold even if it could be done powder won't hold the temp.
why not ceramic coating?
if it's for an intake manifold why not powder it ?
Reply With Quote
  #3 (permalink)  
Old 02-12-2008, 10:59 AM
Newbie
 
Join Date: Jul 2003
Posts: 9
questor
Default Re: PC over manifold paint

It's not the temperature I'm looking for, it's the color. I'm building a Cobra and I painted the side pipes with the manifold paint because it matches the aluminum on my wheels. I want my roll bars to match so I was thinking about using the manifold paint and then putting clear powder over to add some durability.

The manifold paint is good to 2000 degrees and must be cured to a relatively high temperature anyway.

I'm looking for a polished aluminum color and haven't seen a powder in this color.
Reply With Quote
  #4 (permalink)  
Old 02-12-2008, 07:37 PM
Experienced Metal Finisher
 
Join Date: Apr 2004
Posts: 466
jtagger19 is on a distinguished road
Default Re: PC over manifold paint

a picture will work better , polished aluminum looks almost like chrome
and that paint it's a brush or spray paint I don't think it's possible it matches polished aluminum . so in order for it to match you must have like a dull aluminum or anodized aluminum . if this is right you might want to look for chromex ceramic coating wich you can polish to you liking or xtreme chrome powder with clear wich turn to like a reflective silver.

anyway if that paint works to 2000 deg it must be a ceramic based paint and the last time I tried to powder over ceramic it bubled up awfully. it might have been something wrong I did or it might just not work , never tried it again.
still it would be a good project for you to try and let us know.
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
1st Intake Manifold!!! GatorHyde Powder Coating Questions 10 02-02-2008 10:34 PM
Intake Manifold PC ?'s TravisT Powder Coating Questions 4 03-17-2006 07:29 PM
exuast manifold lowgmc94 Powder Coating Questions 2 03-10-2005 02:46 AM
Wanting to paint turbo exhaust manifold and downpipe NCspecV81 Powder Coating Questions 1 12-26-2004 07:45 PM
INLET MANIFOLD pro 100 Metal Polishing Questions 1 01-31-2003 06:50 AM


All times are GMT -4. The time now is 07:21 PM.


Powered by vBulletin® Version 3.7.4
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0
Copyright © Caswell Inc.