Yes you can, might want to test a small piece first. Just remember that the powder you add will only have as good of adhesion as the base powder. I usually use a scotchbrite pad to de-gloss it all and clean it up. Just looking for a color change?
|
|
||||
|
impact or scratch testing.
__________________
SouthWest Powderworx Tyler Nutter 5054803934 www.swpowder.com myspace/swpowder tyler@swpowder.com |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| powder base, wet paint detail, clear powder | FigureLLC | Powder Coating Questions | 6 | 12-22-2007 12:39 AM |
| Powder Powder Everywhere, Newbie | Ikaika | Powder Coating Questions | 15 | 02-28-2007 01:06 PM |
| powder coating over powder coat? | corybarta | Powder Coating Questions | 6 | 08-21-2006 08:15 AM |
| Lolly Pop Powder on a Chrome Surface.. Powder is cracking!! | tattoome5150 | Powder Coating Questions | 5 | 06-18-2005 11:46 PM |