Plating Powder Coating Buffing Anodizing - Caswell Inc. Metal Finishing Forum  

Go Back   Plating Powder Coating Buffing Anodizing - Caswell Inc. Metal Finishing Forum > Powder Coating Questions

Notices

Powder Coating Questions Discussion Board For powder coating questions.

FREE POWDER COATING SYSTEM

Until 9/15 - Buy an HV System, Get a Regular PC System FREE! Two systems for the price of one! (Limited Time - US Customers Only)

HV Powder Coating System

Buy Now


Reply
 
Thread Tools Display Modes
  #31 (permalink)  
Old 05-05-2008, 11:40 AM
Newbie
 
Join Date: May 2007
Posts: 49
GCPJohn is on a distinguished road
Default Re: Moisture Problems???

Quote:
Originally Posted by hjeades View Post
Columbia Coatings sells that gun tip. I have one but have yet to try it out. The ring is plastic, I'm not sure whats it for.
That's where I saw it for sale...try it out, let us know if it really works!
Reply With Quote
  #32 (permalink)  
Old 05-12-2008, 12:29 PM
hjeades's Avatar
Newbie
 
Join Date: Mar 2008
Location: Pekin, Illinois
Posts: 29
hjeades is on a distinguished road
Default Re: Moisture Problems???

I have a small shop in comparison to most of you, so to combat moisture in my air lines I built a cooling coil out of 1/2" type L copper tubbing. The coil comes off of my 1" main line and goes directly to my filter/dryer and coalescing oil filter, and then to my air hose. This made a big difference in the moisture content in my air.
Attached Thumbnails
moisture-problems-dscf1476.jpg  moisture-problems-dscf1474.jpg  
Reply With Quote
  #33 (permalink)  
Old 05-12-2008, 06:49 PM
Newbie
 
Join Date: May 2007
Posts: 49
GCPJohn is on a distinguished road
Default Re: Moisture Problems???

That's a really good idea! Looks cheap to build too!

How's that gun tip working out for you?
Reply With Quote
  #34 (permalink)  
Old 05-14-2008, 08:57 PM
hjeades's Avatar
Newbie
 
Join Date: Mar 2008
Location: Pekin, Illinois
Posts: 29
hjeades is on a distinguished road
Smile Re: Moisture Problems???

Quote:
Originally Posted by GCPJohn View Post
That's a really good idea! Looks cheap to build too!

How's that gun tip working out for you?
Not too bad actually, around a hundred bucks. And it works real good. You can add a small fan to blow accross it if needed.

I have some projects that I am getting ready so I can coat them, so I will let you know about the tip this weekend if not sooner.

Harley

Last edited by hjeades; 05-14-2008 at 08:59 PM.
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Moisture filter. Where and which do I buy? krisnet55 Powder Coating Questions 6 01-14-2008 02:55 PM
regulators and moisture/oil separators defed Powder Coating Questions 6 08-20-2007 11:52 PM
problems krymis Powder Coating Questions 2 01-29-2007 01:45 PM
problems krymis Powder Coating Questions 0 01-28-2007 09:58 PM
Gun Problems johnny933 Powder Coating Questions 2 01-25-2005 10:50 PM


All times are GMT -4. The time now is 11:02 PM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.