I am new to powder coating and I am powder coating my lower forks on my nighttrain. The one fork turned out good the first try the second fork on th other hand not so good. I keep getting a shiny wrinkle instead of the dull,rough texture look. I have tried longer cure,less cure,more powder and less powder. I have always cured at 400 degrees. I have also did the preheating the part. Anyone have any ideas on what to try to fix it?
|
|
|||
|
Wrinkle is hard with a Cup gun. I spray Black wrinkle mainly, have gone through 200Lbs so far this year. If its glossy looking, its Light on powder. Mix the Powder well first before adding into your cup, it will help distrobute the two types of powder in it.
__________________
Dan Pesonen Bandit Powder Coat <<From Powder to Perfection>> Forest Grove, BC Canada Personal motto: "If it ain't broke, modify somethin till it is" |
|
|||
|
All textured powders are sensitive to the right thickness, if no texture, to thin a layer...
|
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Wrinkle finish on non wrinkle powders? | turboxr4ti | Powder Coating Questions | 2 | 01-22-2008 05:45 PM |
| wrinkle black | baz | Powder Coating Questions | 9 | 08-14-2007 09:02 PM |
| Clear over Wrinkle Black?? | ShelbyCSXT | Powder Coating Questions | 1 | 12-03-2006 01:18 PM |
| Engine Pic With Extreme Chrome & Black Wrinkle.. | RNMHRD | Powder Coating Questions | 3 | 12-13-2005 03:25 PM |
| Black Wrinkle | warchild | Powder Coating Questions | 4 | 03-18-2005 06:52 PM |