  #11 (permalink)  
Old 04-10-2008, 03:03 PM
Newbie
 
Join Date: Feb 2008
Posts: 28
osmondmark is on a distinguished road
Default Re: Orange turned out really pale!

Yeah it looks transparent but some of the parts are like that bright orange color. Its just the other half of the parts that came out like that and they have a spot where its mirror. I am starting to think I didn't spray it thick enough...
Reply With Quote
  #12 (permalink)  
Old 04-10-2008, 05:57 PM
nuttyman's Avatar
Metal Finishing Guru
 
Join Date: Sep 2003
Location: Rio Rancho, NM
Posts: 553
nuttyman
Default Re: Orange turned out really pale!

d d dd di diid I stutter?
__________________
SouthWest Powderworx
Tyler Nutter
5054803934
www.swpowder.com
myspace/swpowder
tyler@swpowder.com
Reply With Quote
  #13 (permalink)  
Old 04-10-2008, 06:21 PM
Newbie
 
Join Date: Feb 2008
Posts: 28
osmondmark is on a distinguished road
Default Re: Orange turned out really pale!

Haha I'm lost. But I will try that and see if I applied it to lightly or uneven and post up the results, and ill go from there.

Thanks for the help, you guys are great!
Reply With Quote
  #14 (permalink)  
Old 04-10-2008, 08:49 PM
Newbie
 
Join Date: Feb 2008
Posts: 28
osmondmark is on a distinguished road
Default Re: Orange turned out really pale!

I had trouble tonight with the compressor. I believe there was water in the lines. I am going to get it out and spend a few hours at it tomorrow. I have a bunch of black to do as well so Ill keep you all updated on how it goes.

Thanks
Reply With Quote
  #15 (permalink)  
Old 04-11-2008, 03:04 AM
Newbie
 
Join Date: May 2007
Posts: 49
GCPJohn is on a distinguished road
Default Re: Orange turned out really pale!

That looks exactly like the candy orange from columbia coatings.

Skateboard trucks in candy orange...




Looks the same to me.
Reply With Quote
  #16 (permalink)  
Old 04-11-2008, 10:37 PM
Newbie
 
Join Date: Feb 2008
Posts: 28
osmondmark is on a distinguished road
Default Re: Orange turned out really pale!

I tried it again today with the same results. I did the black after and it turned out perfect, except there was a lot of dust floating around in the shop but I expected that.

I called columbia coatings and they said that it was probably mislabeled and are sending me replacement to try.

Thanks for the help guys!
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
catode turned black fourkbmx Anodizing Questions 1 11-02-2007 12:30 AM
copy cad turned green! R.B. Electroplating Questions 0 07-18-2007 09:38 PM
Anyone used Caswell's Safety Orange or Orange? nuttyman Powder Coating Questions 4 09-02-2005 12:55 PM
my screw up turned out nice corybarta Powder Coating Questions 6 05-09-2005 09:40 PM
Engine turned finishing john morgan Other Metal Finishing Questions 1 03-03-2003 08:31 PM


All times are GMT -4. The time now is 08:02 AM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.