Plating Powder Coating Buffing Anodizing - Caswell Inc. Metal Finishing Forum  

Go Back   Plating Powder Coating Buffing Anodizing - Caswell Inc. Metal Finishing Forum > Powder Coating Questions

Notices

Powder Coating Questions Discussion Board For powder coating questions.

Reply
 
Thread Tools Display Modes
  #1 (permalink)  
Old 05-11-2003, 05:14 PM
Newbie
 
Join Date: Mar 2002
Posts: 2
batuka
Default Powder Coating Pitted Pot Metal

What type of filler would be used to fill pits in pot metal after sand blasting? Bondo is for low-temp applications. Would Epoxy do? I bought some chrome and clear colors and im re-chroming many parts on my car with powder. Do I have to pre-bake before spraying?
Thanks,
Reply With Quote
  #2 (permalink)  
Old 05-12-2003, 03:44 PM
Newbie
 
Join Date: May 2003
Posts: 14
fredde
Send a message via MSN to fredde
Default

I have earlier used som "repair putty" after sandblasting some years ago. Can`t remember what the brand was but I will look into it tomorrow at work, to se if I can find something out. Only thing I can remember that it was ordered from UK and that it worked well.
__________________
Did you know that it is possible to use every gram of powder if you recycle when coating, and vapors are almost none !
In a wet paint approx. 80-90 % evaporates into the air. Causing stress on the enviroment !
1 kg. of powder can cover approx. 10-12 m3
1 litre. of wet paint covers approx. 2-3 m3
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
*** WE ARE GIVING AWAY FREE POWDER COATING *** mcaswell Powder Coating Questions 197 07-08-2008 12:31 PM
powder coating over powder coat? corybarta Powder Coating Questions 6 08-21-2006 08:15 AM
Powder coating on firearms LoneGunman Powder Coating Questions 2 06-15-2006 12:54 PM
New to powder coating ? customandsound Powder Coating Questions 0 06-21-2005 02:00 AM
Non-paint powder coating dshepherd Powder Coating Questions 6 01-26-2004 11:49 AM


All times are GMT -4. The time now is 12:21 AM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.